Quality Requirements Edition 5.0                                                                                  European Enamel Association






            7.27.3 Quality requirements

            Test method                  Requirement                                        Remarks                          Frequency
            4.2  material thickness      min 0.75 mm                                        is not valid for laminated panels   determination during design
            4.3 thickness enamel coating   max. 0.50 mm                                     not applicable if covered with several   S4/AQL 6.5
                                                                                            colour layers in order to achieve special  (when coil production, 1 x per 100 m )
                                                                                                                                                           2
                                                                                            decorative effects
            4.4 cold citric acid         class A                                                                             when taking into production a sig.diff.

                                                                                                                             enamel recipe, but at least 1 x per year
                                                              2
            4.5 boiling citric acid      max. weight loss: 18.5 g/m per 2,5 hours           only for outdoor application     when taking into production a sig.diff.

                                                                                                                             enamel recipe, but at least 1 x per year
            4.9 impact resistance        at 20 N no damage                                                                   when taking into production a sig.diff.

                                         > 2.0 mm diameter after 24 hours                                                    enamel recipe, but at least 1 x a year

            4.10 adherence               min. 2                                             on test sheets may be conform to   in production 1 x a day
                                                                                            EN ISO 28764
                                                           2
            4.12 porosity                max. 10 defects per m                                                               in production min. 1 %
            or:                                                                             only for outdoor application

                                                           2
            4.13 determination of defects   max. 10 defects per m                           in accordance with EN ISO 8289 method B  in production min. 1 %
                                                            2                               in accordance with EN ISO 8289 method A  in production min. 1 %
                                         or max. 5 defects per m
            4.18 scratch resistance      min. 4 N                                                                            when taking into production a sig.diff.
                                                                                                                             enamel recipe (exclusive colour oxides),
                                                                                                                             but at least 1 x a year
            4.26 abrasion resistance     max. 0.1 gram                                      in accordance with ASTM C501     when taking into production a sig.diff.
                                         sandpaper S33/1kg/1000 rotations                                                    enamel recipe (exclusive colour oxides),
                                                                                                                             but at least 1 x a year
            4.28 Steel quality           in accordance with norm EN 10209                   is recommended:                  determination during design

                                                                                            DC01EK / DC04EK / DC04ED